Key Features
Inconel® 600 offers the following key features:
Good Oxidation Resistance
Good Corrosion Resistance at high temperatures
**High temperature static applications
Typical Applications
Inconel® 600 is known to be suitable for the following applications:
Furnace Components
Chemical Processing
Food Processing
Nuclear Engineering
Designations
W.Nr. 2.4816
UNS N06600
AWS 010
Specifications
AMS 5665
AMS 5687
ASTM B166
BS 3075 NA 14
BS 3076 NA 14
DTD 328A
QQ-W-390
Chemical Composition
The chemical composition of Inconel® 600 is indicated in the table below:
Alloy Details
Inconel® 600 density, melting point, coefficient of expansion, modulus of rigidity, and elasticity is indicated in the table below:
Density
Melting Point
Coefficient of Expansion
Modulus of Rigidity
Modulus of Elasticity
8.47 g/cm³
1413 °C
13.3 μm/m °C (20 – 100 °C)
75.6 kN/mm²
206 kN/mm²
0.306 lb/in³
2575 °F
7.4 x 10-6 in/in °F (70 – 212 °F)
10965 ksi
29878 ksi
Heat treatment of finished parts
The typical heat treatment of Inconel® 600:
Condition as supplied by AWI
Type
Temperature
Time
Cooling
Annealed or Spring Temper
Stress Relieve
460 °C (860 °F)
1hr
Air
Properties
The typical mechanical properties of Inconel® 600:
Annealed
Approx. tensile strength
<900 N/mm²
<131 ksi
Approx. operating temperature depending on load** and environment
-200 to +1000 °C
-330 to +1830 °F
Spring Temper
Approx. tensile strength
900 – 1450 N/mm²
131 – 210 ksi
Approx. operating temperature depending on load** and environment
-200 to +1000 °C
-330 to +1830 °F
Slight magnetism may occur below 120 °C (184 °F)
The above tensile strength ranges are typical. If you require different please ask.
Key Features
Inconel® 600 offers the following key features:
Good Oxidation Resistance
Good Corrosion Resistance at high temperatures
**High temperature static applications
Typical Applications
Inconel® 600 is known to be suitable for the following applications:
Furnace Components
Chemical Processing
Food Processing
Nuclear Engineering
Designations
W.Nr. 2.4816
UNS N06600
AWS 010
Specifications
AMS 5665
AMS 5687
ASTM B166
BS 3075 NA 14
BS 3076 NA 14
DTD 328A
QQ-W-390
Chemical Composition
The chemical composition of Inconel® 600 is indicated in the table below:
Alloy DetailsInconel® 600 density, melting point, coefficient of expansion, modulus of rigidity, and elasticity is indicated in the table below:
|
|---|
Heat treatment of finished parts
The typical heat treatment of Inconel® 600:
| Condition as supplied by AWI | Type | Temperature | Time | Cooling |
|---|---|---|---|---|
| Annealed or Spring Temper | Stress Relieve | 460 °C (860 °F) | 1hr | Air |
| Annealed | ||
|---|---|---|
| Approx. tensile strength | <900 N/mm² | <131 ksi |
| Approx. operating temperature depending on load** and environment | -200 to +1000 °C | -330 to +1830 °F |
| Spring Temper | ||
|---|---|---|
| Approx. tensile strength | 900 – 1450 N/mm² | 131 – 210 ksi |
| Approx. operating temperature depending on load** and environment | -200 to +1000 °C | -330 to +1830 °F |
Contact us